Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 173 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 130 - 173 °C
266 - 343 °F
Average value: 157 °C Grade Count:57
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..