Deflection Temperature at 1.8 MPa (264 psi) 80.6 °C
177 °F
ASTM D648
Americas Styrenics MC3650 High Heat Crystal Polystyrene
Product CharacteristicsImproved cycle times in hard to fill partsExcellent clarity with slight blue tintFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsHousewaresConsumer..
Deflection Temperature at 1.8 MPa (264 psi) 80.6 °C
177 °F
ASTM D648
Americas Styrenics STYRON® 693 High Heat Crystal Polystyrene
Product CharacteristicsHigh heat resistanceHigh tensile strengthHigh stiffnessFood Contact CompliantUL Classification 94 HBTypical ApplicationsPackaging/Foam disposablesConsumer electronicsInformati..
Deflection Temperature at 1.8 MPa (264 psi) 80.6 °C
177 °F
ASTM D648
Americas Styrenics STYRON® 478 High Impact Polystyrene
Product CharacteristicsGood glossExcellent balance of flow and stiffnessFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsAppliancesMedicalHousewaresConsumer electronicsIn..
Deflection Temperature at 1.8 MPa (264 psi) 80.6 °C
177 °F
ASTM D648
Westlake Plastics Crystat® ABS (anti-static)
Semitransparent, inherently anti-static material available in roll stock or thin gauge sheet. Its strength and clarity make it excellent for thermoforming.Information provided by Westlake Plastics...