Americas Styrenics STYRON® 478 High Impact Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Americas Styrenics LLC
Trade Name STYRON®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Americas Styrenics STYRON® 478 High Impact Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product CharacteristicsGood glossExcellent balance of flow and stiffnessFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsAppliancesMedicalHousewaresConsumer electronicsInformation provided by AmericasStyrenics LLC.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength at Break 25.5 MPa
3700 psi
ASTM D638
Tensile Strength 29.6 MPa
4300 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Tensile Modulus 2.00 GPa
290 ksi
ASTM D638
Flexural Strength 39.3 MPa
5700 psi
ASTM D790
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
compression molded; ASTM D256
1.07 J/cm
2.00 ft-lb/in
injection molded; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.6 °C
177 °F
ASTM D648
Vicat Softening Point 102 °C
216 °F
ASTM D1525
Copyright © lookpolymers.com All Rights Reserved