Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | |
Plastcom SLOVAMID 6 GF 65 PA6, 65% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ISO 75 |
Nilit FRIANYL B63 BR90 Nylon 6.6 for injection molding, 90% bronze filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ISO 75 |
Nilit FRIANYL B63 W-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | Unannealed; ASTM D648 |
PolyOne Bergamid™ XP6042701 Polyamide 6 (Nylon 6) Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3.5 sec Cycle Time: 18 to 60 secInformation provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ISO 75 |
Nilit FRIANYL B63 GV40 Nylon 6 for injection molding, 40% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ISO 75 |
Nilit FRIANYL B63 GV50 Nylon 6 for injection molding, 50% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | Unannealed; ISO 75-2/C |
Pasargad Polymer Peyvand Pasamid 3P-H1130W Nylon 6, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ASTM D648 |
Lavergne VYPET VNT 335 PET 35% Glass - Mineral Reinforced Vypet VNT 335 is a 35% glass/mineral reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional stabilityT.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | |
LATI Latamid 6 H2 G/50 PA 6, 50% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | |
LATI Later 4 K/30 PBT, 30% Carbon Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplasti.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics ULTEM HU1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Thermocomp JF003L PES LNP* Thermocomp* JF003L is a compound based on Polyethersulfone (PES) containing Glass Fiber. Characteristics of this grade are Low Extractable.This data was supplied by SABIC-IP for the Americas r.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | Unannealed; ASTM D648 |
Teknor Apex Beetle® 140 BH Nylon 66, Glass Bead Reinforced Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | Unannealed; ASTM D648 |
Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced Notes: Impact Modified; Reinforced with 13% Glass Fibers; Synergistic compound exhibiting impact strength and dimensional stability Features: Good Dimensional stability; Good Processability; Heat St.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | As molded; ASTM D648A |
Sumitomo Bakelite North America E 3938A Hardware Grade Epoxy Fiberglass reinforced epoxy molding compound with excellent dimensional stability, good strength and excellent electrical insulation properties.Information provided by Vyncolit, a Sumitomo Bak Group.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ISO 75/Af |
Solvay TECHNYLSTARâ„¢ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, DRY Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, heat and UV stabilized, characterized by a high fluidity of the melt, for injection molding.Available in: Europe Product Applic.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ISO 75 |
Polyram RamSter PF310G6 PBT Alloy, 30% Glass Fiber, UV Stabilized 30% Glass fiber reinforced PBT alloy, low warp properties, UV stabilized for injection molding.Information provided by Polyram. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ASTM-D648 |
Toyobo VYLOPET® EMC320R Polyester Resin VYLOPET® is a polyester resin developed specifically for injection molding. Polyester resins have excellent heat resistance, rigidity, chemical resistance, and electric properties. Grade EMC320R ha.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ISO 75-1/-2 |
DSM Akulon® K224-G0 (Dry) 50% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ISO 75-1/2 |
Bond Laminates TEPEX® dynalite 102-RGUD600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate Within the TEPEX® composite laminate, Polyamide 6 is a resin known for its toughness, stiffness, abrasion resistance, heat and chemical resistances. Roving E-Glass fibers have an excellent impact .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ASTM Test |
BASF Petra® 130 BK-112 30% Glass Filled PET Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ISO 75 |
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry) Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ASTM D648 |
Ashley Polymers Ashlene® 630-25G Nylon 6, 25% Glass Reinforced Nylon 6, 25% glass reinforced resin.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ASTM D648 |
Chem Polymer Chemlon 233 G Nylon 6, 33% Glass Fiber Reinforced A 33% glass fiber reinforced nylon 6 offering excellent high temperature performance, dimensional stability, tensile strength and impact resistance.Data provided by the manufacturer, Chem Polymer. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | HDT/A; ISO 75-2 |
Akro-Plastic Akromid® B3 GF 35 (2473) PA 6 Dry, 35% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | HDT/A; ISO 75-2 |
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Dry, 40% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ISO 75 |
Gharda Chemicals GAFONE™ 3430GF PES, Glass Fiber-Reinforced
(discontinued **) Glass fiber reinforced granules for injection molding. With lower viscosity for molding intricate cross sections.Characteristics: Very high rigidityGood dielectric propertiesHigh mechanical strengt.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ISO 75-2/AF |
Addiplast Addinyl B2 V40 Nylon 6, 40% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BG-50 FC PA6-GF50 Product description: Grilon BG-50 FC is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 FC has the following important properties: Short cycle timesExcellent surfac.. |