Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 163 - 215 °C | 325 - 419 °F | Average value: 187 °C Grade Count:17 |
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 204 - 215 °C | 400 - 419 °F | Average value: 208 °C Grade Count:17 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 53.0 - 215 °C | 127 - 419 °F | Average value: 165 °C Grade Count:41 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |