Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 163 - 215 °C
325 - 419 °F
Average value: 187 °C Grade Count:17
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum ..
Deflection Temperature at 1.8 MPa (264 psi) 204 - 215 °C
400 - 419 °F
Average value: 208 °C Grade Count:17
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a..
Deflection Temperature at 1.8 MPa (264 psi) 53.0 - 215 °C
127 - 419 °F
Average value: 165 °C Grade Count:41
Overview of materials for Polytrimethylene Terephthalate (PTT)
This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val..