Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 247 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 CM40 HS 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: Natural .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 247 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF40 L 40% Milled Glass Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Comp.. |