Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 255 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 225 - 255 °C
437 - 491 °F
Average value: 239 °C Grade Count:12
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
Deflection Temperature at 1.8 MPa (264 psi) 78.0 - 255 °C
172 - 491 °F
Average value: 228 °C Grade Count:137
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Deflection Temperature at 1.8 MPa (264 psi) 75.0 - 255 °C
167 - 491 °F
Average value: 176 °C Grade Count:10
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Deflection Temperature at 1.8 MPa (264 psi) 246 - 255 °C
475 - 491 °F
Average value: 249 °C Grade Count:3
Overview of materials for Nylon 63, 35% Glass-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app..