Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 |
Plaskolite Optix® CA-1000 IG Clear High Impact Acrylic Resin High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin offers the best impact resista.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Geloy XTWM200 ASA ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Europe-Africa-Middle East) Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Geloy FXTW30CP ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | |
Polimeri Europa SINKRAL C433/M3 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,EG,095-08-16-15 Special low gloss grade for extrusion and calendering, with high mattness and medium impact resist.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | annealed; ASTM D648 |
Kleerdex Vinyloy™ 102 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Recycled capped FR sheetApplications: Vinyloy 102 sheet is capped sheet that can be used to substitute effectively for ABS and other grades of thermoplastic sheet for your thermoforming needs.Featur.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® FG133F1 NC010 Nylon 66
(Unverified Data**) Zytel® FG133F1 NC010 is a nucleated PA 66. It has been developed for consideration into applications such as parts for the food industry.Information provided by DuPont |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C @Thickness 6.40 mm |
172 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa HIPS-5197 High Impact Polystyrene Features:UL 94 HB @ 1.6mmExcellent balance propertiesHigh mechanical strengthGood heat stabilityColor tailor-made for clientsApplications:Injection moldingGas assistant moldingTV & Audio housingElec.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | annealed; ASTM D648 |
KYDEX® V Acrylic/PC Thermoplastic Sheet Utility sheetApplications: Can be used to substitute effectively for utility grade thermoplastics. It is very appropriate for hidden parts and painted parts and/or where fire retardancy is not requ.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | unannealed; ASTM D648 |
KKPC Kuhmo HI 425 E Extrusion Molding HIPS Key features: Cold-resistant Extrusion. Common Uses: Refrigerator inner liners, door liners, disposable cups, food packaging sheet, wrapping films, trays, washing machinesHIPS is a functional resin .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | annealed; ASTM D648 |
KYDEX® 6200 Thermoplastic Sheet Fire rated sheet for mass transitApplications: Dashboards, seatbacks, armrests, tray tables, window reveals, cabin linersFeatures: Kydex 6200 is a proprietary, high performance thermoplastic sheet. .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP RBG16I PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RBG16I is a compound based on Nylon 66 resin containing Glass Bead, Graphite. Added features of this material include: High Impact. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER PC+Polyester, UV Stabilized, Transparent |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ISO 75 |
Styrolution PS 454N HIPS Styrolution PS 454N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Good balance of toughness, high flow, and heat resistanceHigh gloss.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM Test |
Styrolution Terluran® GP-22 ABS Terluran GP-22 is an easy flowing grade of ABS for injection molding with high resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF and.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C @Thickness 3.20 mm |
172 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL PVX0800 PPE NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 |
Supreme Petrochem SC 201LV General Purpose Polystyrene CharacteristicsHigh molecular weight grade Good flow properties along with good mechanical strength Easy process ability with good mold release propertiesProcessing Injection moldingApplicationsSuit.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ISO 75-1, 2 |
Polyplastics Duracon® WR-01 Acetal Co-polymer (POM), Chlorine water resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D648 |
Eastman Tenite Propionate 383A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ISO 75-1/-2 |
Covestro Bayblend® FR 3005 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeeasy-flow gradeVicat/B 120 temperature = 95 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (2.0 mm)no j.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 |
Denka TE-10 Transparent Resin Polymer (MABS resin) ABS "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® FG133F1 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66 with Developed for Food Contact Applications Zytel FG133F1 NC010 is a nucleated PA 66. It has been developed for consideration into applications such as parts for the food .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | unannealed; ISO 75 |
Chi Mei Polylac® PA-758R ABS - Transparent Transparent, Chemical Resistant |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM-D648 |
Braskem PCD 0440 HECO Polypropylene Heterophasic Copolymer PCD 0440 is a medium melt flow rate heterophasic copolymer with high impact strength. This resin is designed for steel pipe coating (SPC) and injection molding. Its applications include: automotive.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 |
Adell AS-10 Nylon 66, General Purpose Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | |
BASF Polystyrol® 2710 Impact Grade Polystyrene (Europe) Special high-impact grade for refrigerators and the packaging sector. Particularly resistant to stress cracking.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 |
Plaskolite West Optix® CA-1000 IG Clear High Impact Acrylic Resin High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin is suited for Gamma irradiatio.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics XYLEX X8300CL PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester, UV Stabilized, Transparent, OQ Quality |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | annealed; ASTM D648 |
Kleerdex Kydex® 150 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Class I/A rated thermoplastic sheetApplications: Interior ductwork and chutes, laboratory hoods, shower/tub shrouds, acoustical applications, decorative ceilings, abuse resistant surfacing for count.. |