Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 257 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 220 - 257 °C
428 - 495 °F
Average value: 245 °C Grade Count:15
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Deflection Temperature at 1.8 MPa (264 psi) 254 - 257 °C
490 - 495 °F
ASTM D648
Clariant Renol PA1SP0019 Nylon 66/PPS Alloy, 20% Glass, 20% Mineral
Data provided by Clariant Masterbatches