Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 137 °C
122 - 278 °F
Average value: 74.1 °C Grade Count:99
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..