Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.05 - 1.48 g/cc
0.0379 - 0.0535 lb/in³
Average value: 1.13 g/cc Grade Count:123
Filler Content 25.0 - 32.0 %
25.0 - 32.0 %
Average value: 29.4 % Grade Count:64
Water Absorption 0.0100 - 0.0400 %
0.0100 - 0.0400 %
Average value: 0.0236 % Grade Count:11
Linear Mold Shrinkage 0.00600 - 0.0212 cm/cm
0.00600 - 0.0212 in/in
Average value: 0.0113 cm/cm Grade Count:105
Linear Mold Shrinkage, Transverse 0.00850 - 0.0211 cm/cm
0.00850 - 0.0211 in/in
Average value: 0.0150 cm/cm Grade Count:19
Melt Flow 0.700 - 230 g/10 min
0.700 - 230 g/10 min
Average value: 13.1 g/10 min Grade Count:106
Ash 28.0 - 32.0 %
28.0 - 32.0 %
Average value: 29.9 % Grade Count:13
28.0 - 28.0 %

@Temperature 900 - 900 °C
28.0 - 28.0 %

@Temperature 1650 - 1650 °F
Average value: 28.0 % Grade Count:1
Mechanical Properties Metric English Comments
Hardness, Rockwell M 49.0 - 100
49.0 - 100
Average value: 67.0 Grade Count:4
Hardness, Rockwell R 45.0 - 100
45.0 - 100
Average value: 79.2 Grade Count:20
Hardness, Shore D 64.0 - 82.0
64.0 - 82.0
Average value: 72.1 Grade Count:16
Tensile Strength, Ultimate 13.0 - 36.0 MPa
1890 - 5220 psi
Average value: 26.0 MPa Grade Count:91
Tensile Strength, Yield 15.0 - 38.0 MPa
2180 - 5510 psi
Average value: 27.4 MPa Grade Count:45
Elongation at Break 3.00 - 250 %
3.00 - 250 %
Average value: 21.5 % Grade Count:66
>= 100 %

@Temperature 60.0 - 90.0 °C
>= 100 %

@Temperature 140 - 194 °F
Average value: 100 % Grade Count:1
Elongation at Yield 2.70 - 80.0 %
2.70 - 80.0 %
Average value: 8.40 % Grade Count:63
5.00 - 6.00 %

@Temperature 60.0 - 90.0 °C
5.00 - 6.00 %

@Temperature 140 - 194 °F
Average value: 5.50 % Grade Count:1
Modulus of Elasticity 1.50 - 3.79 GPa
218 - 550 ksi
Average value: 2.57 GPa Grade Count:39
0.500 - 1.10 GPa

@Temperature 60.0 - 90.0 °C
72.5 - 160 ksi

@Temperature 140 - 194 °F
Average value: 0.800 GPa Grade Count:1
Flexural Yield Strength 20.0 - 88.0 MPa
2900 - 12800 psi
Average value: 46.6 MPa Grade Count:74
Flexural Modulus 1.40 - 4.10 GPa
203 - 595 ksi
Average value: 2.51 GPa Grade Count:119
2.60 - 3.70 GPa

@Temperature -20.0 - -20.0 °C
377 - 537 ksi

@Temperature -4.00 - -4.00 °F
Average value: 3.15 GPa Grade Count:2
Izod Impact, Notched 0.149 - 2.40 J/cm
0.280 - 4.50 ft-lb/in
Average value: 0.528 J/cm Grade Count:67
0.300 - 1.00 J/cm

@Temperature -40.0 - 0.000 °C
0.562 - 1.87 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 0.512 J/cm Grade Count:3
Izod Impact, Unnotched 2.51 - 13.3 J/cm
4.70 - 25.0 ft-lb/in
Average value: 4.72 J/cm Grade Count:12
Izod Impact, Notched (ISO) 2.70 - 40.0 kJ/m²
1.28 - 19.0 ft-lb/in²
Average value: 13.1 kJ/m² Grade Count:5
2.10 - 2.10 kJ/m²

@Temperature -40.0 - -40.0 °C
0.999 - 0.999 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 2.10 kJ/m² Grade Count:1
Charpy Impact Unnotched 2.50 J/cm² - NB
11.9 ft-lb/in² - NB
Average value: 5.62 J/cm² Grade Count:31
1.10 - 999.9 J/cm²

@Temperature -40.0 - -20.0 °C
5.24 - 4759 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 2.83 J/cm² Grade Count:25
Charpy Impact, Notched 0.200 - 3.50 J/cm²
0.952 - 16.7 ft-lb/in²
Average value: 0.743 J/cm² Grade Count:54
0.0300 - 0.600 J/cm²

@Temperature -30.0 - -20.0 °C
0.143 - 2.86 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.289 J/cm² Grade Count:43
Gardner Impact 0.565 - 21.7 J
0.417 - 16.0 ft-lb
Average value: 4.47 J Grade Count:22
5.53626 - 5.53626 J

@Temperature -30.0 - -30.0 °C
4.08334 - 4.08334 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 6.89 J Grade Count:1
7.23 - 7.23 J

@Temperature -23.0 - -23.0 °C
5.33 - 5.33 ft-lb

@Temperature -9.40 - -9.40 °F
Average value: 6.89 J Grade Count:2
7.23 - 7.23 J

@Thickness 3.18 - 3.18 mm
5.33 - 5.33 ft-lb

@Thickness 0.125 - 0.125 in
Average value: 6.89 J Grade Count:2
Thermal Properties Metric English Comments
CTE, linear 48.6 - 100 µm/m-°C
27.0 - 55.6 µin/in-°F
Average value: 77.2 µm/m-°C Grade Count:10
Melting Point 150 - 182 °C
302 - 360 °F
Average value: 159 °C Grade Count:19
Deflection Temperature at 0.46 MPa (66 psi) 54.0 - 144 °C
129 - 291 °F
Average value: 119 °C Grade Count:97
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 137 °C
122 - 278 °F
Average value: 74.1 °C Grade Count:99
Vicat Softening Point 52.0 - 192 °C
126 - 378 °F
Average value: 110 °C Grade Count:62
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:55
Oxygen Index 21.0 %
21.0 %
Average value: 21.0 % Grade Count:6
Glow Wire Test 550 - 750 °C
1020 - 1380 °F
Average value: 728 °C Grade Count:32
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
Average value: 1.00e+16 ohm-cm Grade Count:3
Dielectric Strength 19.7 - 24.0 kV/mm
500 - 610 kV/in
Average value: 22.3 kV/mm Grade Count:5
Comparative Tracking Index 600 V
600 V
Average value: 600 V Grade Count:3
Processing Properties Metric English Comments
Processing Temperature 193 - 227 °C
380 - 440 °F
Average value: 210 °C Grade Count:3
Nozzle Temperature 200 - 232 °C
392 - 450 °F
Average value: 220 °C Grade Count:15
Melt Temperature 170 - 279 °C
338 - 534 °F
Average value: 222 °C Grade Count:70
Mold Temperature 15.0 - 80.0 °C
59.0 - 176 °F
Average value: 49.8 °C Grade Count:71
Drying Temperature 51.7 - 100 °C
125 - 212 °F
Average value: 75.4 °C Grade Count:58
Moisture Content 0.0100 - 0.200 %
0.0100 - 0.200 %
Average value: 0.0669 % Grade Count:18
Injection Pressure 2.76 - 120 MPa
400 - 17400 psi
Average value: 66.5 MPa Grade Count:59