Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 287 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 56.0 - 142 °C
133 - 287 °F
Average value: 81.1 °C Grade Count:143
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..