Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 36.7 °C
98.0 °F
ASTM D648
ExxonMobil LLDPE LL 8360.29 Linear Low Density Polyethylene Resin
Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui..
Deflection Temperature at 1.8 MPa (264 psi) 36.7 °C
98.0 °F
ASTM D648
ExxonMobil LLDPE LLP 8360.29 Linear Low Density Polyethylene Resin
Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui..