Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 366 °C
690 °F
ASTM D648
Quadrant EPP Duratron® PI D7015G PI Bearing Grade Polyimide (ASTM Product Data Sheet)