Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 690 °F
Polymer Property :
Deflection Temperature at 1.8 MPa (264 psi) =
690 °F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
366
°C
690
°F
ASTM D648
Quadrant EPP Duratron® PI D7015G PI Bearing Grade Polyimide (ASTM Product Data Sheet)