Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 37.6 °C | 99.7 °F | ASTM D648 |
ExxonMobil HD 6510 Injection Molding Resin
(discontinued **) HD 6510 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a wide ra.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 37.6 °C | 99.7 °F | ASTM D648 |
ExxonMobil HD 6510.17 Injection Molding Resin
(discontinued **) HD 6510 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a wide ra.. |