Deflection Temperature at 1.8 MPa (264 psi) 37.6 °C
99.7 °F
ASTM D648
ExxonMobil HD 6510 Injection Molding Resin  (discontinued **)
HD 6510 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a wide ra..
Deflection Temperature at 1.8 MPa (264 psi) 37.6 °C
99.7 °F
ASTM D648
ExxonMobil HD 6510.17 Injection Molding Resin  (discontinued **)
HD 6510 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a wide ra..