Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 49.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 42.0 - 49.0 °C
108 - 120 °F
ISO-R 75 Method A
Hippe PE 300 Polyethylene
Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall..
Deflection Temperature at 1.8 MPa (264 psi) 43.0 - 49.0 °C
109 - 120 °F
ASTM D648
3D Systems Accura® 40 Plastic for SLA® Systems
40 Accura "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsHigh temperature testing:Automotive "under-the-hood" partsIntake manifoldsLighting components a..