Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ASTM D495 |
Nylene® PX3422 Nylon 6, Impact Extrusion Grade Dry as molded. Film Grade. Nylene PX3422 is a heat stabilized, high impact modified nylon resin designed for maximum toughness with minimum sacrifice in tensile strength and melting point. PX3422 .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Quadrant EPP Borotron® UH PE-UHMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75 method A |
Quadrant EPP Cestilene™ HD 1000 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | 120°C/h; ISO 75/1 |
Polykemi AB SCANFILL BOTTLE BY45C2 Blow Molding Grade Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Quadrant EPP TIVAR® 1000 EC PE-UHMW + specific additives (ISO Data) TIVAR 1000 EC is a PE-UHMW grade containing specific additives rendering this material a lower surface resistivity than TIVAR 1000 antistatic, improving electrical conductivity and UV-resistance |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Quadrant EPP TIVAR® 1000 PE-UHMW, virgin (ISO Data) TIVAR 1000 exhibits a very well balanced property profile. It combines a very good wear and abrasion resistance with an outstanding impact strength, even at temperatures below -200°C. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data) TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufa.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Quadrant EPP TIVAR® Cleanstat PE-UHMW + specific additives (ISO Data) TIVAR CleanStat is a PE-UHMW grade for use in food processing and pharmaceutical industries. It exhibits static dissipative properties and has a food contact compliant composition. Very good wear an.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Quadrant EPP TIVAR® DS PE-UHMW + additives (ISO Data) TIVAR DS is a modified PE-UHMW with extremely high molecular weight. The latter in combination with a particular manufacturing process result in a PE-UHMW grade with superior wear and abrasion resis.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Quadrant EPP TIVAR® MD PE-UHMW + metal detectable additive (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains a metal detectable additive which does hardly affect the inherent PE-UHMW key properties. TIVAR MD presents excellent toughne.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Quadrant EPP TIVAR® SuperPlus PE-UHMW + specific additives (ISO Data) TIVAR SuperPlus is a wear optimised, partially cross-linked PE-UHMW material with extremely high degree of polymerisation for use in most demanding applications and environments. When used for drain.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Polymer Industries Polyslick UHMW Rod Polyslick UHMW Rod exhibits all of the durable qualities of our Polyslick UHMW Sheet making it perfect for the application where sheet stock is not suitable. The material is ideally suited for the m.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75-1/-2 |
Polymer Industries Polyslick UHMW Sheet Polyslick UHMW Sheet exhibits the properties of excellent impact strength, abrasion resistance, low coefficient of friction, as well as very good chemical resistance. This industrial grade material .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | Compression Molded; ASTM D648 |
NOVA Chemicals Surpass® RMs539-UG Octene sMDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 - 46.0 °C | 108 - 115 °F | Average value: 43.7 °C Grade Count:6 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 - 47.0 °C | 108 - 117 °F | Average value: 44.3 °C Grade Count:51 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C @Thickness 3.20 mm |
108 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP FX04491H PE LNP LUBRICOMP* FX04491H is a compound based on Polyethylene resin containing Proprietary Fillers. Added features of this material include: Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ASTM D648 |
Lubrizol Stat-Rite® X-5111 Static Control Polypropylene Stat-Rite® X-5111 is a static dissipative Polypropylene alloy. Stat-Rite® X-5111 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ES.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | Method A; ASTM D-648 |
Chevron Phillips Marlex® HMN TR-938/938G Polyethylene; MDPE Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and good flowLong-term UV stabilizationExcellent impact stre.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 - 49.0 °C | 108 - 120 °F | ISO-R 75 Method A |
Hippe PE 300 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ASTM D648 |
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**) Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | |
Arkema Group Rilsan® MA 4420 Nylon 12, Flexible Tubing Grade (Dry) Designation ISO 1874-PA12-HI,EHL,22-003Flexible grade for tubes extrusion. Available color: black. Light and heat stabilized.Flexibility. High burst pressure and impact strength. Fit for use in a wi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ASTM D648 |
ExxonMobil Escorene® HD-8661 HDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness & impact strengthUses: Large agricultural tanks, Industrial products |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ASTM D648 |
ExxonMobil Escorene® HD-8760 HDPE, Rotational Molding Pellets
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness, Good flowUses: Recreational products, Industrial components, RV tanks |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ASTM D648 |
ExxonMobil Escorene® HD-8761 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8700 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8761 is fully formula.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ISO 75 |
BASF Nypel® 2351 HS BK PA6 (Dry) Description: Nypel® 2351 HS BK is a heat stabilized, pigmented black, impact modified PA6 extrusion grade compound. Quality and performance are combines at a lower cost. It is based on recycled PA6.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 °C | 108 °F | ASTM D648 |
ExxonMobil Escorene® HD-8760 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8700 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8760 is fully formula.. |