Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 343 °C | 650 °F | Unannealed; ASTM D648 |
Oxford Polymers PEEK 20GF-Natural PEEK, 20% Glass Fiber Reinforced Product Description: Glass Fiber (20% Reinforced), PEEK, Polyetheretherketone injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Glass fiber Special Chara.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 343 °C | 650 °F | Unannealed; ASTM D648 |
Oxford Polymers PEEK-20CF-Black PEEK, 20% Carbon Fiber Reinforced Product Description: Carbon Fiber (20% Reinforced), PEEK, Polyetheretherketone, injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Carbon fiber Special Ch.. |