Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 92.2 - 106 °C
198 - 223 °F
Average value: 98.1 °C Grade Count:6
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe..
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C
198 °F
ASTM D648
Spartech CamAlloy /ABS Weatherable Sheet
Description: Weatherable SheetInformation provided by Spartech.
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C
198 °F
ASTM D648
Spartech Korad® SP-9011 Cap ABS Sheet
Description: ABS SheetInformation provided by Spartech.
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C
198 °F
ASTM D648
Spartech Panel Pro ABS UV-Resistant Embossed Sheet Specialty Sheet
Description: Specialty SheetInformation provided by Spartech.
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C
198 °F
ASTM D648
Spartech Soft Touch ASA/ABS Co-Extruded Specialty Sheet
Description: Specialty SheetInformation provided by Spartech.
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C
198 °F
ASTM D648
Spartech SP-9010 General Purpose ABS Sheet
Description: ABS SheetInformation provided by Spartech.
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C
198 °F
ASTM D648
Spartech SparAlloy Rigid Foamed ABS Specialty Sheet
Description: Specialty SheetInformation provided by Spartech.
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C

@Thickness 3.17 mm
198 °F

@Thickness 0.125 in
annealed; ASTM D648
Sumitomo Chemical Sumipex® LG2 Acrylic Resin, High Flow
Product CharacteristicsHigh FlowInformation provided by Calsak Corporation
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C
198 °F
Unannealed; ASTM D648
Teknor Apex Chemlon® 212 Nylon 6, Unreinforced
Features: Lubricated, General Purpose; General purpose nylon 6; Slightly tougher and more ductile than nylon 66 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex..
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C
198 °F
ASTM D648
CPC - Vycom Corzan® CPVC Chlorinated PVC
Corzan CPVC is a high heat, corrosion resistant chlorinated polyvinyl chloride (CPVC) sheet. Because of its excellent corrosion resistance at elevated temperatures, it is ideally suited for self-sup..
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C
198 °F
0.125 in bar Annealed 4 hours at 80°C; ASTM D648
Diamond Polymers ABS 3300
Description: General Purpose Utility BlackInformation provided by Diamond Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C
198 °F
0.125 in bar Annealed 4 hours at 80°C; ASTM D648
Diamond Polymers ABS VP-11 SHF
Description: High Flow, Flame Retardant ABSInformation provided by Diamond Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C
198 °F
0.125 in bar Unannealed/Conditioned 40 hours at 23°C; ASTM D648
Diamond Polymers ASA T-120
Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat ResistanceInformation provided by Diamond Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C
198 °F
0.125 in bar Annealed 4 hours at 80°C; ASTM D648
Diamond Polymers ABS VP-11
Description: Flame Retardant ABSInformation provided by Diamond Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C
198 °F
Aclo Accutech ABS ABS831G40L Glass Reinforced
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C
198 °F
Aclo Accutech Polypropylene Copolymer CP0436C20L Calcium Reinforced