Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 70.0 - 106 °C | 158 - 223 °F | Average value: 89.0 °C Grade Count:82 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 92.2 - 106 °C | 198 - 223 °F | Average value: 98.1 °C Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 - 106 °C | 172 - 222 °F | Average value: 90.0 °C Grade Count:24 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 - 106 °C | 125 - 223 °F | Average value: 89.2 °C Grade Count:211 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.6 - 106 °C | 105 - 223 °F | Average value: 59.7 °C Grade Count:56 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |