Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Softening Point = 1180 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 1180 °C
2160 °F
Dilatometric @ 10psi
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation
Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty..
Softening Point 1180 °C
2160 °F
Dilatometric @ 10psi
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation
Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty..
Copyright © lookpolymers.com All Rights Reserved