Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 1180 °C | 2160 °F | Dilatometric @ 10psi |
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Softening Point | 1180 °C | 2160 °F | Dilatometric @ 10psi |