Polymer Property : Softening Point = 1200 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 650 °C
1200 °F
Novum Glass Solid Soda-lime Industrial Series Glass Microspheres
Solid soda-lime glass microspheres in colorless powder form. Industrial Series Microspheres are solid glass microspheres (also referred to as soda lime glass beads, glass spheres, or microbeads) us..
Softening Point 650 °C
1200 °F
Novum Glass Solid Soda-lime Technical Series Glass Microspheres
Solid soda-lime glass microspheres in colorless powder form. Technical Series Microspheres are solid glass microspheres that have a narrow particle size distribution. Used for chromatography, colum..
Softening Point 650 °C
1200 °F
Novum Glass Solid Soda-lime Uniform Series Glass Microspheres
Solid soda-lime glass microspheres in colorless powder form. Uniform Series Microspheres are used for controlling a bond line thickness in adhesive bonding. Solid glass microspheres are used in a v..
Softening Point 650 °C
1200 °F
Mo-Sci Corporation GL-0191 Soda-Lime Glass Spheres
Appearance: Solid soda-lime glass beads with light green color in powder formTypical applications of GL0191 beads include: spacer material for gauge control, coating, filler for plastic, retroreflec..
Softening Point 650 °C
1200 °F
Mo-Sci Corporation GL-0191-S Soda-Lime Glass Spheres
Appearance: Solid soda-lime glass microspheres that appear colorlessTypical applications of GL0191S glass microspheres include: grinding, mixing media, filter aids, filter media, and thermal expansi..
Softening Point 650 °C
1200 °F
Mo-Sci Corporation GL-0252 Blue Soda-Lime Glass Spheres
Appearance: Solid soda-lime glass microspheres with light blue color in powder form.Typical applications of GL-0252 glass microspheres include: spacer for gauge control, thermal expansion reduction ..
Softening Point 650 °C
1200 °F
Mo-Sci Corporation GL-0262 Ni Coated Soda-Lime Glass Spheres
Appearance: Solid soda-lime glass microspheres with metallic nickel coatingTypical applications of GL-0262 glass microspheres include: conductive filler for plastic, pigment, and etc.Information pro..
Softening Point 650 °C
1200 °F
Mo-Sci Corporation GL-0275-S Class VI Soda-Lime Spheres
Appearance: Solid soda-lime glass microspheres with light green color in powder form.Typical applications of GL0275-S beads including: high temperature spacer material for gauge control, coating, fi..
Softening Point 650 °C
1200 °F
Mo-Sci Corporation GL-0279 Silver Coated Soda-Lime Glass Spheres
Appearance: Solid soda-lime glass microspheres with metallic silver coating.Typical applications of GL0279 beads including: conductive filler for plastic, pigment, and etc.Information provided by Mo..