Material Notes:
Appearance: Solid soda-lime glass microspheres with light blue color in powder form.Typical applications of GL-0252 glass microspheres include: spacer for gauge control, thermal expansion reduction filler for adhesives and polymers, plus they have the advantage of being colored for visualization.Information provided by Mo-Sci Corporation.
Physical Properties Metric English Comments
Bulk Density 1.30 g/cc
0.0470 lb/in³
of Dry Beads
Density 2.50 g/cc
0.0903 lb/in³
pH 7.8
7.8
in water
Mechanical Properties Metric English Comments
Compressive Strength 274.93 MPa
39875 psi
Thermal Properties Metric English Comments
CTE, linear 9.00 µm/m-°C

@Temperature 30.0 - 300 °C
5.00 µin/in-°F

@Temperature 86.0 - 572 °F
Softening Point 650 °C
1200 °F
Component Elements Properties Metric English Comments
Al2O3 1.0 - 3.0 %
1.0 - 3.0 %
CaO 9.0 - 10 %
9.0 - 10 %
Fe2O3 3.0 - 5.0 %
3.0 - 5.0 %
MgO 1.0 - 3.0 %
1.0 - 3.0 %
Na2O 10 - 15 %
10 - 15 %
SiO2 60 - 70 %
60 - 70 %
Descriptive Properties Value Comments
Approximate Coating Thickness 600-1000 angstroms
Chemical Composition 6-8%
Co3O4
Users viewing this material also viewed the following: