Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 115 °C
239 °F
JIS K-2531
Unitika elitel UE3230 Polyester, Flake
Adhesive agent, Resin modifierUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink binde..
Softening Point 115 °C
239 °F
Flow beginning temperature
Wanhua Chemical Wanthane® WHT-6226 TPU Hot-Melt Adhesive
Wide range of activation temperature, fast crystallization rate, outstanding bonding strength for fabrics, leathers, plastics & rubbers, wood, etc.Information provided by Wanhua Chemical Group Co., ..
Softening Point 115 °C
239 °F
Zeon Chemicals Quintone® G115 Aliphatic Hydrocarbon Resin
C5/C9 type (piperylene and dicyclopentadiene precursor).Information provided by Zeon Chemicals L.P.
Softening Point 115 - 135 °C
239 - 275 °F
Beijing Ranger Chem SM-607 Solid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Softening Point 115 °C
239 °F
Flow beginning temperature
Wanhua Chemical Wanthane® WHT-6233 TPU Hot-Melt Adhesive
Wide range of activation temperature, fast crystallization rate, outstanding bonding strength for fabrics, leathers, plastics & rubbers, wood, etc.Information provided by Wanhua Chemical Group Co., ..
Softening Point 115 - 120 °C
239 - 248 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 151 Linear Thermoplastic Polyurethane  (discontinued **)
PEARLBOND® 125/H is polycaprolactone-based thermoplastic polyurethane, supplied in form of colourless or slightly yellowish, translucid pellets, combining a low hardness with excellent low-temperat..
Softening Point 115 °C
239 °F
Flow beginning temperature
Wanhua Chemical Wanthane® WHT-6232 TPU Hot-Melt Adhesive
Wide range of activation temperature, fast crystallization rate, outstanding bonding strength for fabrics, leathers, plastics & rubbers, wood, etc.Information provided by Wanhua Chemical Group Co., ..