Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Advanced Materials PEARLBOND® 151 Linear Thermoplastic Polyurethane  (discontinued **)

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLBOND® 151 Linear Thermoplastic Polyurethane  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PEARLBOND® 125/H is polycaprolactone-based thermoplastic polyurethane, supplied in form of colourless or slightly yellowish, translucid pellets, combining a low hardness with excellent low-temperature flexibility.Applications: PEARLBOND® 151 is used for textile coating for making shoe-stiffeners (toe puffs & counters), by extrusion or sintering process.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
DIN 53.479
Brookfield Viscosity 100 - 400 cP
100 - 400 cP
RVT (15% in MEK); MQSA 40 A
Melt Flow 15 - 25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
15 - 25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
DIN 53.735
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
DIN 53.505
Tensile Strength, Yield 20.0 MPa
2900 psi
DIN 53.504
Elongation at Break 750 %
750 %
DIN 53.504
Thermal Properties Metric English Comments
Melting Point 140 - 145 °C
284 - 293 °F
MQSA 70 A
Softening Point 115 - 120 °C
239 - 248 °F
MQSA 70 A