Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 1700 °C | 3090 °F | |
Saint-Gobain Quartzel® Fused Quartz Textiles Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, non-porous, continuous, amorphous, ultra pure silica glass. It is ava.. |