Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 600 °C | 1110 °F | |
Mo-Sci Corporation GL-0176 Barium-Titanate Glass Spheres Appearance: Solid glass microspheres with light yellow color in powder form.Typical applications of GL0176 beads include: high temperature spacer material for gauge control, coating, filler for plas.. |
|||
Softening Point | 600 °C | 1110 °F | |
Mo-Sci Corporation GL-0275-B Class VI Barium-Titanate Glass Spheres Appearance: Solid glass microspheres with light yellow color in powder form.Typical applications of GL0275-B beads including: high temperature spacer material for gauge control, coating, filler for .. |
|||
Softening Point | 600 °C | 1110 °F | |
3M S42XHS Glass Bubbles 3M™ Glass Bubbles S42XHS are high-strength additives for polymers made from a water-resistant and chemically stable sodalime-borosilicate glass. These hollow glass microspheres can be compounded wi.. |
|||
Softening Point | 600 °C | 1110 °F | |
3M Scotchlite™ S60/10000 Glass Bubbles High-strength polymer additives made from a water-resistant and chemically-stable soda-lime-borosilicate glass. These hollow glass microspheres can be used as a low density filler material ideal for.. |
|||
Softening Point | 600 °C | 1110 °F | |
3M XLD3000 Glass Bubbles 3M™ Glass Bubbles XLD3000 are high-strength additives for polymers made from a water-resistant and chemically stable soda-lime-borosilicate glass. These hollow glass bubbles can be compounded with .. |
|||
Softening Point | 600 °C | 1110 °F | |
Mo-Sci Corporation GL-0175 Barium-Titanate Glass Spheres Appearance: Solid glass microspheres with light yellow color in powder form.Typical applications of GL0175 beads include:: high temperature spacer material for gauge control, coating, filler for pla.. |