Material Notes:
3M™ Glass Bubbles S42XHS are high-strength additives for polymers made from a water-resistant and chemically stable sodalime-borosilicate glass. These hollow glass microspheres can be compounded with a variety of polymers to reduce the overall thermal conductivity of the composite. These composites can be coated or incorporated into deep sea oil pipelines to improve the flow assurance properties of the system. The high strength of S42XHS glass bubbles can withstand both the high processing pressure of polymer extrusion and the pressure of seawater in many applications. The S42XHS glass bubbles have isostatic crush strengths of 8000 psi with a minimum of 90% survival.Information provided by 3M
Physical Properties Metric English Comments
Density 0.420 g/cc
0.0152 lb/in³
Volatiles 0.40 %
0.40 %
Particle Size 25 µm
25 µm
diameter
pH 9.5
9.5
5% loading in water
Thermal Properties Metric English Comments
Thermal Conductivity 0.140 W/m-K

@Temperature 50.0 °C
0.972 BTU-in/hr-ft²-°F

@Temperature 122 °F
Softening Point 600 °C
1110 °F
Descriptive Properties Value Comments
Alkalinity 0.5 milliequivalents/gram
Appearance White, powdery
unaided eye
Shape Hollow spheres with thin walls