Thermal Properties Metric English Comments
Boiling Point 165 °C
329 °F
Solvay Specialty Polymers Galden® D02TS PFPE Fluid
Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat..
Boiling Point 165 °C

@Pressure 0.101 MPa
329 °F

@Pressure 14.7 psi
3M Fluorinert™ FC-40 Electronic Liquid
3M™ Fluorinert™ Liquid FC-40 is a non-conductive, thermally and chemically stable fluid ideal for single phase heat transfer fluid applications, especially in the electronics and semiconductor ind..
Boiling Point 165 - 166 °C
329 - 331 °F
BASF N,N-Dimethylacetamide
Formula: C4H8NOCAS: 127-19-5Description: Dimethylacetamide is a colorless to yellow liquid with a faint, specific amine-like odor. It is miscible with water and other organic substances.Synonyms: D..