Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 165 °C | 329 °F | |
Solvay Specialty Polymers Galden® D02TS PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
Boiling Point | 165 °C @Pressure 0.101 MPa |
329 °F @Pressure 14.7 psi |
|
3M Fluorinert™ FC-40 Electronic Liquid 3M™ Fluorinert™ Liquid FC-40 is a non-conductive, thermally and chemically stable fluid ideal for single phase heat transfer fluid applications, especially in the electronics and semiconductor ind.. |
|||
Boiling Point | 165 - 166 °C | 329 - 331 °F | |
BASF N,N-Dimethylacetamide Formula: C4H8NOCAS: 127-19-5Description: Dimethylacetamide is a colorless to yellow liquid with a faint, specific amine-like odor. It is miscible with water and other organic substances.Synonyms: D.. |