Boiling Point 158 °C
316 °F
Initial; ASTM D86
ExxonMobil Varsol™ 1 Non-dearomatized Fluid
Appearance: Clear/Transparent LiquidAvailability: Central America, North America and South AmericaInformation provided by ExxonMobil
Boiling Point 158 °C
316 °F
Initial; ASTM D86
ExxonMobil Varsol™ 40 Non-dearomatized Fluid
Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and EuropeInformation provided by ExxonMobil
Boiling Point 158 - 159 °C
316 - 318 °F
BASF Isopropanolamine
Formula: C3H9NOCAS: 78-96-6Description: Isopropanolamine is a colorless to yellowish liquid with an amine-like odor. It is miscible in water.Synonyms: 1-Amino-2-propanol, Monoisopropanolamin, 1-Ami..