BASF Isopropanolamine

Category Fluid
Manufacturer BASF
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Isopropanolamine.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Formula: C3H9NOCAS: 78-96-6Description: Isopropanolamine is a colorless to yellowish liquid with an amine-like odor. It is miscible in water.Synonyms: 1-Amino-2-propanol, Monoisopropanolamin, 1-Amino-2-hydroxypropane, 1-Methyl-2-aminoethanol, 2-Hydroxy-1-propylamine, 2-Hydroxypropanamine, 2-HydroxypropylaminApplications: Intermediate used in the production of Dyes, Lubrification oils, Corrosion inhibitor, Detergents and Cutting fluidInformation provided by BASF
Physical Properties Metric English Comments
Density 0.962 g/cc
0.0348 lb/in³
Molecular Weight 75.1 g/mol
75.1 g/mol
Thermal Properties Metric English Comments
Melting Point 2.00 °C
35.6 °F
Boiling Point 158 - 159 °C
316 - 318 °F
Flash Point 71.0 °C
160 °F
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
DIN 51 777
Descriptive Properties Value Comments
Assay >99%
Color <20
APHA, DIN EN 1557
Composition Diisoproanolamine
<0.1%
Ignition Temperature 335°C