Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 2080 °C | 3780 °F | |
Indium Corp. 4N Commercial Indium Metal Indium is a versatile metal with unique physical properties.Indium has one of the widest liquid temperature ranges of any metal.Indium has a low vapor pressure, making it ideal for high vacuum appli.. |
|||
Boiling Point | 2080 °C | 3780 °F | |
Indium Corp. 5N Commercial Indium Metal Indium is a versatile metal with unique physical properties.Indium has one of the widest liquid temperature ranges of any metal.Indium has a low vapor pressure, making it ideal for high vacuum appli.. |
|||
Boiling Point | 2080 °C | 3780 °F | |
Indium Corp. 3N Commercial Indium Metal Indium is a versatile metal with unique physical properties.Indium has one of the widest liquid temperature ranges of any metal.Indium has a low vapor pressure, making it ideal for high vacuum appli.. |