Material Notes:
Indium is a versatile metal with unique physical properties.Indium has one of the widest liquid temperature ranges of any metal.Indium has a low vapor pressure, making it ideal for high vacuum applications.Indium is a soft, pliable and malleable, even down to cryogenic temperaturesRelatively low toxicityIndium is a bright shiny metal that forms a thin (80 - 100 angstroms) protective oxide layer. It is used as a decorative trim coating metallization on plastics for appliance and automobile trim.Indium effectively reduces the melting point in solder alloys and fusible alloys.Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Density 7.30 g/cc
0.264 lb/in³
Thermal Properties Metric English Comments
Melting Point 157 °C
315 °F
Boiling Point 2080 °C
3780 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 0.0060 %
0.0060 %
Cadmium, Cd 0.0060 %
0.0060 %
Copper, Cu 0.0042 %
0.0042 %
Indium, In 99.9 %
99.9 %
Iron, Fe 0.00030 %
0.00030 %
Lead, Pb 0.0086 %
0.0086 %
Nickel, Ni 0.00050 %
0.00050 %
Silver, Ag 0.00010 %
0.00010 %
Thallium, Tl 0.00020 %
0.00020 %
Tin, Sn 0.0185 %
0.0185 %