Polymer Property : Boiling Point = 410 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Boiling Point 210 °C

@Pressure 0.101 MPa
410 °F

@Pressure 14.7 psi
LG Chemical NPG Flake Neopentyl Glycol
NPG is a diol with two hydroxyl groups located in the 1,3-position on the primary carbon atom. Additionally, it has two methyl groups instead of the usual two hydrogen atoms on the a-carbon atom. It..
Boiling Point 210 °C
410 °F
760 mm Hg
Dow Hydroxypropyl Acrylate
Hydroxypropyl Acrylate for high performance coatings. (Clear, colorless liquid)Information provided by Dow
Boiling Point 210 °C
410 °F
BASF Formamide
Formula: CH2NOCAS: 75-12-7Description: Formamide is a colorless liquid, with an odorless odor. It is miscible in water.Synonyms: MethanamideApplications: Intermediate used in the production of Crop..
Boiling Point 210 °C
410 °F
BASF Lupragen® N 400 Trimethylamineoethylethanolamine
Formula: C7H18N2OCAS: 2212-32-0Description: Trimethylaminoethylethanolamine is a colorless to light yellow liquid, with an amine-like odor. It is miscible with water and other organic solvents.Syno..
Boiling Point 210 °C
410 °F
BASF NEOL® Neolpentylglycol Flakes
Formula: C5H12O2CAS: 126-30-7Description: Neolpentylglycol (NEOL) flakes are colorless with a sweetish odor.Synonyms: Neopentanediol, 2,2-Dimethyl-1,3-propanediol, 1,3-Dihydroxy-2,2-dimethylpropane,..
Boiling Point 210 °C
410 °F
BASF NEOL® Neolpentylglycol Pure Liquid
Formula: C5H12O2CAS: 126-30-7Description: Neolpentylglycol (NEOL) pure liquid is a colorless melt, with a sweetish odor. Synonyms: Neopentanediol, 2,2-Dimethyl-1,3-propanediol, 1,3-Dihydroxy-2,2-dim..