Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Boiling Point = 6480 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Boiling Point 3580 °C
6480 °F
American Elements Zirconium Nanoparticles
General DescriptionZirconium (Zr) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Zirconium Particles are typically 10-40 nanometers (nm) with ..
Copyright © lookpolymers.com All Rights Reserved