Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering F50A Fluorosilicone Rubber Blue Fluorosilicone, 45-55 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain.Applications: Excellent heat resistance and low temperature flexib.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering F80R Fluorosilicone Rubber Red Fluorosilicone, 76-85 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification DTD5583A Grade 80.Applications: |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering N60C Nitrile Rubber Nitrile Butadiene Rubber (NBR). High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet British Gas Specification BGC/PS/LC6 Class "C", 55-65 IRHD. Approval ref.: 31/6.1... |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering N70J Nitrile Rubber Peroxide cured Nitrile Butadiene Rubber (NBR), 66-75 °IRHD. Copolymer of acrylonitrile and butadiene. To meet DTD 5594A standard for resistance to mineral oils.Applications: Excellent resistance i.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering N70N Nitrile Rubber Nitrile Butadiene Rubber (NBR) 66-75 °IRHD. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD5595A Grade 70.Applications: Synthetic rubber resistant to petrole.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering N70V Nitrile Rubber Nitrile Butadiene/PVC Rubber, 65-75 °IRHD. Copolymer of acrylonitrile and butadiene blended with PVC.Applications: Excellent resistance in sealing applications against petroleum and mineral based f.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering N80L Nitrile Rubber Nitrile Butadiene Rubber, 75-85 °IRHD. Low acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet ASTM D2000 line call-out M6BG814, A14, B14, EO14, EO34, F17.Applications: T.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering N85U Nitrile Rubber Nitrile Butadiene Rubber (NBR) 75-95 °IRHD. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD458A Grade B1 (specification inactive for new design).Applications.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering N90K Nitrile Rubber Peroxide cured Nitrile Rubber, 85-95 °IRHD. Copolymer of acrylonitrile and butadiene. ASTM designation = NBR. ISO designation = NBR. ASTM D2000/SAE J200 line call-out M7BG910, B14, EA14, EF11, EF21.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering R50Z Natural Rubber Natural Rubber, 45-55 °IRHD. Formulated to meet BS1154 Grade Z50. In accordance with BS1154 this material is based on high-quality plantation (Hevea) rubber, reinforced with carbon black.Applicati.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering R80Z Natural Rubber Natural Rubber, 75-85 °IRHD. Formulated to meet BS1154 Grade Z80. In accordance with BS1154 this material is based on high-quality plantation (Hevea) rubber, reinforced with carbon black.Applicati.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S50A Silicone Rubber Blue Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain.Applications: Excellent heat resistance and low temperature flexibility. Use.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S60E Silicone Rubber Red iron oxide filled, Phenyl Silicone Rubber, 55-65 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aerospace Speci.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S60R Silicone Rubber Red Silicone 55-65 °IRHD. Diesel cylinder liner ring grade. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excell.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S60T Silicone Rubber Translucent Silicone Rubber, 55-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United St.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S60X Silicone Rubber Red Silicone Rubber, 55-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Specially compounded to provide .. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S60Z Silicone Rubber Grey Silicone Rubber, 55-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States Fo.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S65A Silicone Rubber Low Compression Set, Blue Silicone Rubber, 65-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Low compre.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S65B Silicone Rubber Low Compression Set, Black Silicone Rubber, 65-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Low compr.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S65W Silicone Rubber Low Compression Set, Off-white Silicone Rubber, 65-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Low c.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S65Y Silicone Rubber Golden Yellow, Silicone 55-65 °IRHD. Diesel liner ring grade. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and low temperature flexibility combined with low compression set.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S70G Silicone Rubber Green Silicone Rubber, 66-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States F.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering S80N Silicone Rubber Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aircraft Materials Specification DTD5582A Grade .. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering Z75L Hydrogenated NBR Compound Peroxide Cured, Hydrogenated Nitrile Rubber, 75-85 °IRHD. Low acrylonitrile content (ACN = 17%).Applications: Specially compounded for service in low-temperature applications. High strength and ex.. |
|||
Flash Point | >= 300 °C | >= 572 °F | |
Precision Polymer Engineering Z85B Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Rubber, 76-85 °IRHD. Medium acrylonitrile content (ACN =36%). ASTM designation = HNBR. ASTM D2000 line call-out MDH814, A26, B36, EO16, EO36, F14.Applications.. |
|||
Flash Point | 300 - 340 °C | 572 - 644 °F | |
LG Chemical KEYFLEX BT 1068D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Flash Point | 300 - 340 °C | 572 - 644 °F | |
LG Chemical KEYFLEX BT 1163D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Flash Point | 300 °C | 572 °F | DIN EN 22592 |
Lucobit Luxbit® Hard Bitumen Luxbit is a hard bitumen with improved properties of earlier high vacuum bitumen (HVB). Luxbit is specially suitable for the production of asphalt screed.Information provided by Lucobit AG |