Flash Point 126 °C
259 °F
ASTM D92
ExxonMobil Vacmul O 3 D
Vacmul O 3 D is a non-staining honing oil recommended for rough and finish honing of safety razor blades. It is suitable for light duty high speed applications and for use in large volume circulatio..
Flash Point 126 °C
259 °F
ASTM D92
ExxonMobil Vacmul O 3 D
Vacmul O 3 D is a non-staining honing oil recommended for rough and finish honing of safety razor blades. It is suitable for light duty high speed applications and for use in large volume circulatio..
Flash Point 126 °C
259 °F
Pensky Martens closed cup
Dow VORANATE™ T-80 toluene diisocyanate (TDI)