Precision Polymer Engineering N80M Nitrile Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering N80M Nitrile Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nitrile Rubber, 75-85 °IRHD. Meets British Standard BS2751 BA80. Medium acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. ASTM designation = NBR. ISO designation = NBR.Applications: Excellent resistance to petroleum based oils and fuels. Excellent compression set, tear and abrasion resistance. Good water resistance but poor against ozone and weather.
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
°IRHD; ASTM D1415
89
89
°IRHD, +5 change after 70 hours @ 70°C; ASTM D1415
Tensile Strength, Yield 12.5 MPa
1810 psi
ASTM D412
13.75 MPa
1994 psi
10% change after 70 hours @ 70°C; ASTM D412
Elongation at Break 150 %
150 %
ASTM D412
165 %
165 %
10% change after 70 hours @ 70°C; ASTM D412
Compression Set 20 %
20 %
24 hours @ 70°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
-15.0 °C
5.00 °F
Temperature at which stiffness does not exceed 70 Mpa
Flash Point >= 300 °C
>= 572 °F
Copyright © lookpolymers.com All Rights Reserved