Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 216 °C | 421 °F | ASTM D92 |
ExxonMobil 15M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Flash Point | 216 °C | 421 °F | ASTM D92 |
ExxonMobil Teresstic 32 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Flash Point | 216 °C | 421 °F | |
ChevronTexaco Canopus® 32 Texaco Canopus oils deliver value through:High resistance to forming emulsions due to excellent water separating characteristics.Long lubricant life provided by outstanding stability.Good lubricant .. |
|||
Flash Point | 216 °C | 421 °F | ASTM D92 |
ChevronTexaco ISO 100 Utility Oil LVI FeaturesChevron Utility Oils LVI are general purpose lubricants. Chevron Utility Oils LVI are light-colored oils that possess excellent natural low pour points, along with low carbon-forming tendenc.. |
|||
Flash Point | 216 °C | 421 °F | ASTM D92 |
ExxonMobil 15M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Flash Point | 216 °C | 421 °F | ASTM D92 |
ExxonMobil Febis K Series 32 Exxon Febis K Series oils are premium quality lubricants designed to satisfy the strictest requirements of machine tool slideways. Their multi-functional performance makes them suitable for combined.. |
|||
Flash Point | >= 216 °C | >= 421 °F | |
ExxonMobil Mobil DTE 724 Oil Mobil DTE 724 Oil was developed for higher-output gas turbines such as the General Electric Heavy Duty Gas Turbine Frame 7000. Mobil DTE 724 Oil offers excellent thermal and oxidative stability, and.. |
|||
Flash Point | 216 °C | 421 °F | ASTM D92 |
ExxonMobil Mobil Vactra 1 The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a.. |
|||
Flash Point | 216 °C | 421 °F | ASTM D92 |
ExxonMobil Teresstic 32 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Flash Point | 216 °C | 421 °F | COC |
ConocoPhillips Conoco® El Mar® Grade 30 Mid Ash Supreme Oil Conoco® El Mar Mid Ash Supreme is a premium quality, mid-ash, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately to highly turbocharged 4-stroke cycle natura.. |
|||
Flash Point | 216 °C | 421 °F | |
ConocoPhillips Hydroclear® 10W-30 Super All Season and Super Motor Oil Description: Conoco Hydroclear Super All Season and Super Motor Oils, formulated with premium base stocks, lubricate domestic and imported passenger cars, sport-utility vehicles, light-duty trucks, .. |
|||
Flash Point | 216 °C | 421 °F | |
ChevronTexaco Alcaid® 220 Texaco Alcaid® oils deliver value through:Low pour points that permit oils to remain fluid at subzero temperatures.Ready separation from water, an important property where severe moisture condition.. |
|||
Flash Point | 216 °C | 421 °F | ASTM D92 |
ExxonMobil 526 Mobil SHC 500 Series Mobil SHC 500 Series oils are supreme performance hydraulic oils formulated from synthesised, wax-free hydrocarbon base fluids combined with a carefully engineered super-stabilised additive system. .. |
|||
Flash Point | 216 °C | 421 °F | |
ConocoPhillips Hydroclear® 10W-40 Super All Season and Super Motor Oil Description: Conoco Hydroclear Super All Season and Super Motor Oils, formulated with premium base stocks, lubricate domestic and imported passenger cars, sport-utility vehicles, light-duty trucks, .. |
|||
Flash Point | 216 °C | 421 °F | ASTM D92 |
ExxonMobil 526 Mobil SHC 500 Series Mobil SHC 500 Series oils are supreme performance hydraulic oils formulated from synthesised, wax-free hydrocarbon base fluids combined with a carefully engineered super-stabilised additive system. .. |
|||
Flash Point | 216 °C | 421 °F | ASTM D92 |
ExxonMobil Febis K Series 32 Exxon Febis K Series oils are premium quality lubricants designed to satisfy the strictest requirements of machine tool slideways. Their multi-functional performance makes them suitable for combined.. |
|||
Flash Point | >= 216 °C | >= 421 °F | |
ExxonMobil Mobil DTE 724 Oil Mobil DTE 724 Oil was developed for higher-output gas turbines such as the General Electric Heavy Duty Gas Turbine Frame 7000. Mobil DTE 724 Oil offers excellent thermal and oxidative stability, and.. |
|||
Flash Point | 216 °C | 421 °F | ASTM D92 |
ExxonMobil Mobil Vactra 1 The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a.. |
|||
Flash Point | 216 °C | 421 °F | |
ChevronTexaco Alcaid® 100 Texaco Alcaid® oils deliver value through:Low pour points that permit oils to remain fluid at subzero temperatures.Ready separation from water, an important property where severe moisture condition.. |