Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 338 °C | 640 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® T7109-19 Electrically Insulating Epoxy Paste Material Description: A flexible, thermally conductive, electrically insulating epoxy paste designed for low stress and heat dissipation applications. It is an alternative to EPO-TEK® T7109-17, de.. |