Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Decomposition Temperature 338 °C
640 °F
Degradation Temperature
Epoxy Technology EPO-TEK® T7109-19 Electrically Insulating Epoxy Paste
Material Description: A flexible, thermally conductive, electrically insulating epoxy paste designed for low stress and heat dissipation applications. It is an alternative to EPO-TEK® T7109-17, de..