Polymer Property : Decomposition Temperature = 350 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Decomposition Temperature 320 - 350 °C
608 - 662 °F
Thermal Stability via TGA : beginning - and at 1% weight loss in air
Solvay Specialty Polymers Solef® 31008 PVDF Copolymer  (discontinued **)
Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General ..
Decomposition Temperature 300 - 350 °C
572 - 662 °F
Thermal Stability via TGA : beginning - and at 1% weight loss in air
Solvay Specialty Polymers Solef® 3108/0903 Anti-static PVDF Compound  (discontinued **)
Key features of this grade: Anti-static, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crystall..
Decomposition Temperature 330 - 350 °C
626 - 662 °F
Thermal Stability via TGA : beginning - and at 1% weight loss in air
Solvay Specialty Polymers Solef® 20810 PVDF Copolymer  (discontinued **)
Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta..