Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 402 °C | 756 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® EV2002 Silver-filled, electrically conductive, flexible epoxy Material Description: Silver-filled, electrically conductive, flexible epoxyInformation Provided by Epoxy Technology |
|||
Decomposition Temperature | 402 °C | 756 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® OE120 Two Component Epoxy Material Description: A two component, opaque epoxy, designed for fiber optics packaging applications. It is a black-colored version of EPO-TEK 353ND-T. It has a high Tg for resisting elevated ope.. |