Epoxy Technology EPO-TEK® OE120 Two Component Epoxy

Category Polymer , Thermoset , Epoxy
Manufacturer Epoxy Technology
Trade Name EPO-TEK®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Epoxy Technology EPO-TEK® OE120 Two Component Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material Description: A two component, opaque epoxy, designed for fiber optics packaging applications. It is a black-colored version of EPO-TEK 353ND-T. It has a high Tg for resisting elevated operating temperatures found in medical fiber optics or hybrid-microelectronic applications.Information Provided by Epoxy Technology
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
Part B
1.21 g/cc
1.21 g/cc
Part A
Particle Size <= 20 µm
<= 20 µm
Viscosity 12000 - 16000 cP

@Temperature 23.0 °C
12000 - 16000 cP

@Temperature 73.4 °F
20 rpm
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Tensile Modulus 3.18 GPa
461 ksi
Storage
Shear Strength >= 13.8 MPa
>= 2000 psi
Lap
>= 35.2 MPa
>= 5100 psi
Die
Thermal Properties Metric English Comments
CTE, linear 28.0 µm/m-°C
15.6 µin/in-°F
Below Tg
121 µm/m-°C
67.2 µin/in-°F
Above Tg
Maximum Service Temperature, Air 250 °C
482 °F
Continuous
350 °C
662 °F
Intermittent
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Continuous
-55.0 °C
-67.0 °F
Intermittent
Glass Transition Temp, Tg >= 90.0 °C
>= 194 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 402 °C
756 °F
Degradation Temperature
Electrical Properties Metric English Comments
Volume Resistivity >= 6.00e+12 ohm-cm
>= 6.00e+12 ohm-cm
Dielectric Constant 3.47

@Frequency 1000 Hz
3.47

@Frequency 1000 Hz
Dissipation Factor 0.010

@Frequency 1000 Hz
0.010

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 2.00 min

@Temperature 120 °C
0.0333 hour

@Temperature 248 °F
minimum
10.0 min

@Temperature 100 °C
0.167 hour

@Temperature 212 °F
minimum
20.0 min

@Temperature 80.0 °C
0.333 hour

@Temperature 176 °F
minimum
Pot Life 210 min
210 min
Shelf Life 6.00 Month

@Temperature 25.0 °C
6.00 Month

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Amber
Part B
Black
Part A
Consistency Smooth thixotropic paste
Mix Ratio By Weight 10:1
Number of Components Two
Weight Loss 0.07%
200°C
0.38%
250°C
1.12%
300°C
Users viewing this material also viewed the following: