Thermal Properties Metric English Comments
Decomposition Temperature 412 °C
774 °F
Degradation Temperature
Epoxy Technology EPO-TEK® 353ND High Temperature Epoxy
Product Description: EPO-TEK® 353ND is a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applications. It is one of the most popular EPO-TEK® bra..
Decomposition Temperature 412 °C
774 °F
Degradation Temperature
Epoxy Technology EPO-TEK® H81A Epoxy
Material Description: A two component, gold-filled, electrically and thermally conductive epoxy designed for hybrid microelectronic and semiconductor packaging.Information Provided by Epoxy Technolo..